Patterning Sn-based EUV resists with low-energy electrons (1910.02511v1)

Published 6 Oct 2019 in physics.app-ph and cond-mat.mtrl-sci

Abstract: Extreme Ultraviolet (EUV) lithography is the newest technology that will be used in the semiconductor industry for printing circuitry in the sub-20 nm scale. Low-energy electrons (LEEs) produced upon illumination of resist materials with EUV photons (92 eV) play a central role in the formation of the nanopatterns. However, up to now the details of this process are not well understood. In this work, a novel experimental approach that combines Low-Energy Electron Microscopy (LEEM), Electron Energy Loss Spectroscopy (EELS), and Atomic Force Microscopy (AFM) is used to study changes induced by electrons in the 0-40 eV range in thin films of molecular organometallic EUV resists known as tin-oxo cages. LEEM-EELS spectroscopic experiments were used to detect surface charging upon electron exposure and to estimate the electron landing energy. AFM post-exposure analyses revealed that irradiation of the resist with LEEs leads to the densification of the resist layer associated to carbon loss. The same chemical processes that yield densification render the solubility change responsible for the pattern formation in the lithographic application. Remarkably, electrons as low as 1.2 eV are able to induce chemical reactions in the Sn-based resist. Based on the thickness profiles resulting from LEE exposures in the 3-48 mC/cm 2 dose range, a simplified reaction model is proposed where the resist undergoes sequential chemical reactions, yielding first a sparsely cross-linked network, followed by the formation of a denser cross-linked network. This model allows us to estimate a maximum reaction volume on the initial material of 0.15 nm 3 per incident electron in the energy range studied, which means that less than 10 LEEs per molecule on average are needed to turn the material insoluble and thus render a pattern.

Summary

We haven't generated a summary for this paper yet.